LANTHANIDE
Oxides and Ceramics...
|
-
-
- Présentation
:
-
- Here a is large file on
lanthanide oxides (also called " rare earth " oxides)
and their uses in ceramics with a particular attention
to their "unreal" colouring action as compared to the
traditional colouring materials currently used.
-
- Four articles make it up :
- - a general technological
description of the oxides of lanthanides, article by
Smart2000 (France).
- - a complete review of
current toxicological knowledge pertaining to the use
of rare earths, article written by Édouard
Bastarache (Quebec).
- - an article on the
colouring of transparent glazes going from cone 5-6 to
cone 10-11, article written by David Pier (USA).
- - an article on the
experimentation of lanthanide oxides in
macro-crystalline glazes containing zinc, article by
Smart2000 (France)..
- This very comprehensive
presentation concerning the various aspects of glazes
coloured by lanthanide oxides is unique by the
richness of its content and the revelation of these
resources so little used in traditional ceramics
nowadays.
-
- Smart2000 invites all of
those who would be ready to share their experience in
this field to communicate their articles and documents
to widen this field of knowledge so little explored
and still ignored by many ceramists
- (Contact :
smart2000@wanadoo.fr).
-
- Access to
files :
-
- LANTHANIDES
and
CERAMICS,
technological article by
Smart2000 (France)
-
- RARE
EARTHS,
TOXICOLOGY,
article by Edouard
Bastarache (Quebec)
-
- LANTHANIDE
COLOURANTS,
"Exciting new transparent
glaze colors using lanthanide colorants", article by
David Pier (U.S.A).
-
- LANTHANIDE
COLOURING OXIDES in ZINC CRYSTALLINE
glazes,
article by Smart2000
(France).
-
-
-
- Smart2000.fr
©
Avril 2003
-
FRANCE
- Écrit
et documenté par le propriétaire du site
// Contact : Smart2000@wanadoo.fr
- Document
pour CONSULTATION PRIVÉE uniquement - Toute
reproduction totale ou partielle est
interdite
-
-
-
-
- Smart2000.fr
le site
dédié aux passionnés de
céramique
-
- Smart2000
- FRANCE sur https://smart2000.fr/
-
- This
entire page Copyright © 2003-2023, All Rights
Reserved.
- Les
textes et les photos restent la
propriété de leur auteurs, ils ne
peuvent être réutilisés sans un
accord préalable. Nous
consulter.
|